| Mass per unit area | EN 1849-2 | 160 g/m2 |
| Thickness | EN 1849-2 | 0.5 mm |
| Straightness | EN 1848-2 | conforming |
| Water vapour transmission (Sd) | EN 1931/EN ISO 12572 | 0.1m |
| Maximum tensile fore MD/CD | EN 12311-1 | 280 / 220 N/50mm |
| Elongation MD/MC | EN 12311-1 | 50 / 60% |
| Resistance to tearing MD/MC | EN 12310-1 | 180 / 200 N |
| Water-tightness | EN 1928 | Class W1 |
| UV resistance | EN 13859-1 | 4 months |
| Temperature resistance | - | -40/+100˚c |
| Reaction to fire | EN 13501-1 | class E |
| Resistance to penetration of air | EN 12114 | < 0.o2m3/m2h50Pa |
| After ageing: | - | - |
| • maximum tensile force MD/CD | EN 13859-1 | 260 / 200 N/50 mm |
| • water-tightness | EN 13859-1 | Class W1 |
| • elongation MD/CD | EN 13859-1 | 40 / 50% |
| Flexibillity at low temperature | EN 1109 | -40C |
| Dimensional stability | EN 1107-2 | <2% |
| Thermal conductivity (λ) | - | 0.4 W/mK |
| Specific heat | - | 1800 J/kgK |
| Density | - | approx. 370 kg/m3 |
| Water vapour resistance factor (μ) | - | approx. 160 |
| Recommended installation pitch | - | >13 degrees |
| Driving rain test | TU Berlin | passed |
| VOC emissions | - | 0 % (class A+) |
| Joint strength | EN 12317-2 | >200 N/50 mm |